Chris, you could take the boards out of storage and apply voltage to re-form the dielectric. Since the capacitors are rated at a higher voltage than they would see in the circuit, you might have to use some ingenuity to make sure (if you wanted to) they are being restored to equivalent to new condition. Also, you might use higher voltage rated capacitors than you require for functionality, figuring that degradation of the dielectric, even after 10 years, would still leave you with a part of sufficient voltage rating. Capacitor manufacturers could tell you if that approach makes sense. Lou Hart ---------- From: Christophe CROCOMBETTE[SMTP:[log in to unmask]] Sent: Friday, January 26, 2001 8:42 AM To: [log in to unmask] Subject: [TN] Storage of Electrolytic caps Hi, Does anybody have some info on the recommended storage duration of electrolytic capacitors (and how to extend it) ? I read from manufacturers data that the recommandation is usually not to exceed 2-3 years (the alumine layer is gradually destroyed by the electrolyte when the cap does not work). My problem is that I want to store some boards for over 10 years, with elec. caps. Is there another solution than storing the boards without the parts ? Thanks Chris --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------