Hi there Ken. Have you tried peelable resist to cover these pads? What I do is have a slot put into any pads that are to be wave soldered without components. If your software cannot do this to a pad (and Mine cannot) what I do is create the slot in the Gerber data. You can create a rectangle of copper etc & make a Gerber of it. (make it 1mm wide or the solder will jump across it!) Then in GC-Prevue (or similar Gerber viewer) place this rectangle over the pad so that its longest length goes in line with the direction of flow into the wave solder machine. Then have the layer marked as "composite". This creates a slot in the pad. If you have multiple pads to do, copy the rectangle onto all the pads that need it and then create the Gerber,l not forgetting some form of alignment markings. Your PCB suppliers front end chaps should be able to sort the rest (once you tell them what its for!). > Date: Wed, 17 Jan 2001 13:48:19 +0800 > From: Ken Fong <[log in to unmask]> > Subject: Special through hole pad design > > Technetters, > Could anyone advise a design of soldering pad which will not be closed > with > solder during wavesoldering when the hole is not inserted with component, > but it > can form a normal solder joint when a component is inserted through the > hole > with the lead clinched by auto-insertion machine? The board is 1.6mm thick > single sided pcb. Thanks. > > Ken > > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------