Thanks for all the responses regarding the use of silver epoxy and solder coated parts... obviously, not the way to go! I'm still trying to understand the mechanism for increased DC resistance, though. From what I have learned, silver oxides are conductive, so this isn't it. The tin seems to migrate into the epoxy, I assume leaving a lead-rich zone. Is it that the lead oxidizes? Are lead oxides conductive? Can anyone explain? Thanks again, Jim Marsico EDO Electronic Systems Group [log in to unmask] <mailto:[log in to unmask]> -----Original Message----- From: Mike Fenner [SMTP:[log in to unmask]] Sent: Wednesday, January 24, 2001 1:52 PM To: TechNet E-Mail Forum.; Marsico, James Subject: Re: [TN] silver epoxy & solder coated parts I would avoid it. Conventionally: Epoxy has poor adhesion to tin and its alloys The tin/silver interface will give an inter-reaction at the bondline leading to electrical opens although you may retain mechanical adhesion. One/Two years is a long time in this situation especially if you have mechanical stress/vibration or any temperature swings in service. This is very well documented in the literature and you should see something in the Technet archives. More open mindedly: There are some companies working on this and there are now products which claim to have solved this problem, either by using a sort of halfway house product (adhesive with a fusible metal filler basically) or by special undisclosed ingredients/formulations. Contact suppliers for the latest Mike ----- Original Message ----- From: "Marsico, James" <[log in to unmask]> To: <[log in to unmask]> Sent: Tuesday, January 23, 2001 8:34 PM Subject: [TN] silver epoxy & solder coated parts > Hello, Technet... > > Here is an unusual situation. We have to assemble a surface mount assembly > using silver epoxy. Some of the components will be solder coated. I know, > don't bother asking... this is the way it has to be. The good thing is that > this assembly is a prototype for bench-top laboratory use only. There is no > harsh environment and needs to operate 1, maybe 2, years. The question is > does anyone foresee any problems? What happens when one mixes toe two > technologies? > > Thanks, > Jim Marsico > EDO Electronic Systems Group > [log in to unmask] <mailto:[log in to unmask]> > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------