Franklin, Here's a list of what we look for on our Developer. Spray nozzles: Full deflection of all nozzles, no clogs Proper oscillation of manifolds. All nozzles and manifolds in-line and parallel to each other Equipment: No excess solution drag out on exit. i.e. good squeegee effect same on entrance Break Point: 55% -65% of process chamber length. We run a solution of Potassium Carbonate, Shipley's Resolve 211 at 1.0% +/- 0.1% I also recommend a good water soluble defoamer. Avoid the use of glycol based defoamers. You want to avoid the slime that typically can be seen with most defoamers. Rinsing: GOOD rinsing is critical. Preferably, you want a triple cascade counter flow rinse. I cannot say if you would like to use heated rinses, as I have heard conflicting views on whether this would be a good idea. Now with all the specs out of the way, I can say our last DOE showed us that breakpoint is the most critical of all parameters. You can design an experiment around trace width resolution, but you may want to contact your dry film vendor on help with DOE parameters and running conditions. I hope this helps you a bit. Oh one last thing. We had this problem a few weeks ago with opens. Increasing the roll pressure on your resist laminator may help a bit in increasing conformity. Regards, Sean Clinton Process Engineer Sanmina Plant 3 Santa Clara, CA Franklin D Asbell wrote: > Is there anyone out there that recently designed an experiement, or > experiments for identifying best controls for a dry film developer? > > Still working on lifted resist and we want to ensure optimal performance > of all equipment...while most equipment here is pretty straightforward > in that regard, I'm looking for the best series of data or attributes to > evaluate at the developer, thanks... > > And also...hope everyone has a good new year holiday... > > Franklin > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------