In a message dated 12/21/00 3:57:53 PM Eastern Standard Time, [log in to unmask] writes: << I was wondering how you go about putting nomenclature on copper surfaces and subsequently processing thru immersion tin or immersion silver without experiencing nomenclature peel? >> Lisa, We perform legend screen prior to Immersion White Tin (IWT) with no peel issues. Bob Lazzara VP, Marketing & Tech Support Circuit Connect, Inc. (800) 560-9457 --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------