Ken, Are they through hole or SMT? Rick -----Original Message----- From: Ken Patel [mailto:[log in to unmask]] Sent: Tuesday, December 12, 2000 12:06 PM To: [log in to unmask] Subject: [TN] Failure analysis of cap: Type analysis and any lab that can do th e job in San Jose Bay Area Guys, I have caps with current leakage problem. I have few questions in that regards. What kind of test should I perform for failure analysis? What can be the possible causes for the failures? Any lab you guys can recommend in the San Jose Bay area. re, ken patel ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------