For plating tin/lead from fluoroborate baths, what is the current wisdom of using stainless steel baskets for anode balls? Relative strong points of graphite vs. stainless steel? Thank you, Jol Sprowles, Ph.D. Senior Process Engineer Tyco / Electronics / Printed Circuit Group - Stafford Division Phone: (860)684-5881 ext. 263