Lou, While not addressing your original question, why don't you just skim the copper out? Your SPC chart will let you know when to do this. Ryan Grant Advanced Technology Engineer MCMS (208) 898-1145 [log in to unmask] > -----Original Message----- > From: Lou Hart [SMTP:[log in to unmask]] > Sent: Wednesday, December 06, 2000 1:03 PM > To: [log in to unmask] > Subject: [TN] Copper contamination is wave solder > > TechNetters, > > I've made SPC charts to track tin, copper, gold, and antimony in our wave > solder machine. The operator skims dross from the solder pot every > morning. We send a solder sample the first of each month to Kester for > analysis. Over the past 7 months, there has been a monotonic increase in > copper concentration and the past two months have been above the upper > control limit. The copper concentration is still well within spec (0.3%, > if I am correct, according to the relevant IPC standard) at 0.14%, but I > want to make sure we know what is happening. > > Any comments on these observations? Some years back I had charts for a > HASL machine and over perhaps 12 months the semimonthly copper > concentration wandered between 0.21 and 0.24 %. > > Lou Hart > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------