Hi Lon, In the "component manufacturers section" of my website (http://www.smtinfo.net) you'll find some links to the assembly recommendations of several BGA-manufacturers. Kind regards, Daan Terstegge Signaal Communications Unclassified mail Personal Website: http://www.smtinfo.net >>> Lon Weffers <[log in to unmask]> 11/16 12:14 pm >>> Dear Technetters, One of our customers wants to use a BGA with about 500 solderpoints. Type unknown. We never placed a BGA at all. Does someone have usefull information about reflow profiles?. The BGA is going to be placed on a HASL pcb. Thanks in advance, Lon L.D. Weffers Matas Electronics B.V. Technisch directeur Tel: 0499-335050 Fax: 0499-335051 [log in to unmask] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------