Be careful of that type of separators. In our case, we found that the bodies of chip caps about 0.20 inches from the edges were cracked due to the displacement of the fr4 material as the blades travels along the score line. If your components are 'far' away from the edge it may be fine. Try before you buy. Perform your evaluation and tests. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Trevor Goddard Sent: Tuesday, November 07, 2000 10:41 AM To: [log in to unmask] Subject: [TN] PCB Separating Equipment Hi All Does anyone out there use a CAB PCB Separator to depanelize V-scored boards? If so does anyone have a contact for the CAB company or supplier? Actually if anyone has contacts for any other depanelizing equipment it would also be appreciated. Thanks Trevor Goddard, SMT Supervisor XLTEK (905) 829-5300 x 348 [log in to unmask] <mailto:[log in to unmask]> ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------