The listed cure time for the one part Dow Corning 1765 conformal coating is; tack free in 8 minutes, full cure in 24 hours at 25 deg. C Can be force cured at up to 60 Deg. C May not even need the oven in the application stated. Ernie Crump, Raytheon Systems Canada --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------