Yes for the Solder Mask and no to the conformal coating. Thanks [log in to unmask] COM To: [log in to unmask] Sent by: cc: TechNet Subject: Re: [TN] PCB Corrosion <[log in to unmask] ORG> 21/11/00 09:47 Please respond to "TechNet E-Mail Forum."; Please respond to Robisan1 Two Questions: 1) are the conductors coated with solder mask? 2) are you using conformal coating? Susan Mansilla Tech Drt Robisan lab --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------