Stephen, I think you're referring to test methods within Mil-Std-883. Test method 1010 is Temperature Cycle, 1011 is Thermal Shock, and 1008 is Stabilization Bake. If that sounds right, then follow either of these links for the standard. If they don't work, let me know and I can send you a pdf version of the methods (not the whole standard...too big at 8Meg) http://stinet.dtic.mil/str/dodiss4_fields.html http://www.dscc.dla.mil/ Not sure about the EIAJ standard, but here's their web site: http://www.eiaj.or.jp/english/index.htm Glenn > -----Original Message----- > From: Stephen Ayotte [SMTP:[log in to unmask]] > Sent: Wednesday, November 29, 2000 12:07 PM > To: [log in to unmask] > Subject: [TN] Specifications > > Where could I get copies of: > > Mil Std M1010 > Mil Std M1011 > Mil Std M1008 > > EIAJ-IC-121-01 > > Stephen Ayotte, IMD Manufacturing Quality Engineer > Dept. N62V, Bldg. 966-2, Office 2J1309, Mail Drop 967A > > Phone (802) 769-4775, t/l 446-4775, Fax (802) 769-4139 > Pager (802) 878-5386 Pin #4685 - external, 74685 - internal > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------