Hi Brett, Right now we're trying to get rid of baking by putting all our bare boards in a dry storage room. But in unconditioned storage, in a wet climate (we're in the Netherlands), baking the boards is advised by most bare board vendors, especially for polyimide ! Don't know about G-200. Kind regards, Daan Terstegge Unclassified mail Personal Website: http://www.smtinfo.net >>> <[log in to unmask]> 10/26 12:52 pm >>> Fellow Technetters, particularly those of you who assemble. Recently we had some boards made of Isola(allied signal) G-200(BT-Epoxy) exhibit delam during wave solder. These boards were made in week 19-00, wrapped in paper and shelved until week 34-00 when they were assembled. The assembler says nobody bakes boards anymore. My understanding is that G-200 and Poyimide are extremely hydrscopic, more so than standard epoxies, and lab test show that the defective area was high in water content. If this had been the case back in week 19-00 when I leveled them, they would have delamed then. Do you assemblers still bake prior? Should these materials be baked prior to assembly ? How should they be stored and handled ? Steve are you there ? Thanks Guys Brett Austin Nationwide Circuits Inc [log in to unmask] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------