Rick: E-10 and Epsilam-10 are trademarks of 3M for its ceramic filled PTFE substrate. Dave Fish Rick Babyak wrote: > Has anybody heard of epsilam-10 or know the manufacturer of this > material? > > Rick Babyak > Process Engineer > Proto Circuit Inc. > 7 Ascot Parkway > Cuyahoga Falls, OH 44223 > 330-572-3401 Fax:330-572-3434 > [log in to unmask] > > --------------------------------------------------------------------------------- > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF TECHNET > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------