Janice, What temperatures are your wash / rinse cycles? I found white residues routinely with water soluble chemistries and OSP panels following wave solder, and it turned out that my temperatures were set too high. Jon Moore --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------