Hi Rick, Try Pac Tech of Germany, they have semiautomatic and automatic solder ball placement machine using laser reflow method. You can follow the link to visit their website http://www.pactech.de I've included Mr. Thomas Oppert from the Sales & Marketing in this mail. Should you need more information, you may contact him. Cheers 4 now, At 10:59 AM 10/12/2000 -0700, Rick Thompson wrote: >Hi, > >I'm looking for someone who can reball a small quantity of custom ceramic >BGAs. My normal reballer (Six Sigma) can't handle ceramics with less than >1.27mm pitch which these are. Any recommendations for other sources for >this type of service would be appreciated. > >Thanks in advance, > > > >Rick Thompson >Ventura Electronics Assembly >2665A Park Center Dr. >Simi Valley, CA 93065 > >+1 (805) 584-9858 voice >+1 (805) 584-1529 fax >[log in to unmask] > >--------------------------------------------------------------------------------- >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF TECHNET >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional >information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 >ext.5315 >--------------------------------------------------------------------------------- Daniel Woon Assistant Manager, PCBA Department Comacraft Sdn Bhd (A Subsidiary of Dynavest Group-Asia) 2033, Jalan Bukit Minyak, Kawasan Industri Ringan Asas Jaya, 14100 Bukit Mertajam, Penang, Malaysia. Tel : 60-4-5889933 Fax : 60-4-5889953 H/P : 60-19-4706083 Email : [log in to unmask] Website: http://www.dynavest.com.sg --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------