Sorry all I miss-read George's question. -----Original Message----- From: George Gerberick [mailto:[log in to unmask]] Sent: Wednesday, October 11, 2000 6:25 PM To: [log in to unmask] Subject: [TN] Copper measurement We are looking for the least expensive way of measuring total surface copper thickness on a finished circuit board. Typical areas would not be covered by soldermask but may have white tin, ni-au or solder. Equipment I have used in the past was for copper in the hole, not surface. Any suggestions? ---------------------------------------------------------------------------- ----- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------