From: Paul M Fly Hi gang, I have to make a few comments here. The company I work for is now working with a contract manufacturer for our PCB assembly needs. We used to have an in-house assembly operation, but they went out of business a year or two ago. When we had the in-house assembly going we were required to put local fiducials on fine pitch SMT parts. Our definition of fine pitch being less than 25 mils. On a tight board getting those local fiducials in place could be a real problem, but we could generally find a way to make it work. Then our in-house group goes out of business and we are told to use the contract manufacturer. They want us to put local fiducials on regular 50 mil pitch BGAs! Steve I gotta tell you Jim is 150% right, we are being pushed to make boards smaller but at the same time we are getting pressure for local fiducials in addition to global fiducials and thats on parts that our own assembly group could place two years ago using just the global fiducials! Sorry to sound like I'm venting (well maybe I am a little), but this trend I've been seeing is moving in the wrong direction. Jim, to answer your question, yes we have been able to group parts into clusters and share fiducials. We have been given a dimension, (which I imagine varys from vendor to vendor) that we are told as long as the parts all fall within this distance from the fiducial it is ok to share a fiducial with several parts. Thanks for listening, Paul Fly "Stephen R. Gregory" <[log in to unmask]> on 10/05/2000 12:04:35 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to [log in to unmask] To: [log in to unmask] cc: (bcc: Paul M Fly/243609/EKC) Subject: Re: [TN] Fiducials and HDI In a message dated 10/05/2000 9:55:18 AM Central Daylight Time, [log in to unmask] writes: Hi Jim! I'd have to agree with Daan. Very rarely, if ever, have I used local fiducials. As long as there is some good global fiducials, I've never found the need to use Locals...this includes placing 15.7-mil pitch parts and MicroBGA's... -Steve Gregory- > Hi Jim, > > One solution could be to place the local fiducials underneath the components. > Another solution: don't use them. > And do you really need a 0.150 (inch ?) keep out area ? > > Kind regards, > > Daan Terstegge > SMT Centre > Signaal Communications > Unclassified mail > Personal Website: http://www.smtinfo.net > > >>> Jim Kittel <[log in to unmask]> 10/05 3:25 pm >>> > TechNetters, > > With so much emphasis on reducing circuit board feature sizes by use of > micro BGA's, micro lead frames, micro vias, etc. the use of local fiducials > becomes a real burden. For example, our typical fiducial is a 0.048 circle > with a 0.150 keep out area. This keep out area is approaching the size of > flash memories, micro BGA's, 0402 chips, etc. > > Has anyone figured out a way to work around this local fiducial problem? Is > anyone grouping these parts into some kind of symmetric clusters? Any > ideas? > > Jim Kittel ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------