Jim, Is this housing going to be seen by your customer? Would the nickel plating be punctured or chipped off by an engraving pencil? regards, Bev Christian -----Original Message----- From: Marsico, James [mailto:[log in to unmask]] Sent: Wednesday, October 18, 2000 3:23 PM To: [log in to unmask] Subject: [TN] INK MARKING Having trouble ink marking (epoxy ink) on nickel plated housings. Marking comes off during in-line aqueous cleaning process. Any suggestions? Thanks, Jim M. ---------------------------------------------------------------------------- ----- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF TECHNET Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------