Dear Rudy: Aside from the specific gravity (Baume'), I believe the parameters proffered for an ORP/Conductivity/SG controlled cupric system, regardless of the oxidizer employed (chlorine gas, hydrogen peroxide, or sodium chlorate) were sufficiently wide to apply all systems (excluding PCMI applications). Forgive me regarding the Baume' range, as I have become accustomed to working with sodium chlorate regenerated systems. This range would not be inclusive of chlorine gas and hydrogen peroxide regenerated cupric systems. However, sodium chlorate systems do indeed operate at good effeciency within 29 - 31 Baume' range with ORP control. In reading your response, I feel you may have presumed I was advocating a particular method of control. Though it is likely we have opposing viewpoints, I belive the recommendation to take the time to process sample panels at users employing different technologies is valid. Regards, Ted Stern 877-272-1272 "" wrote: > In a message dated 9/29/00 8:07:15 AM Pacific Daylight Time, > [log in to unmask] writes: > > << In terms of cupric chloride > bath chemistry, a comparison of the operating parameters between ORP and > turbidimetric > methods of control is as follows: > > Method of Control ORP Turbidimetric > > Cu (total), g/L 150-180 210-235 > HCl, N 1 - 3 > 0.02-0.04 > Baume' 29 - 31 > 38-40 > >> > > WRONG WRONG AND WRONG! > You can control the etchant to ANY READING in a ORP/acid/Baume' type > controller. That is the beauty of that sort of system, versus the > turbidimetric system, the turbidimetric system defines what your readings > MUST be, whereas the other system allows you to choose what YOU want. > > It is the replenisher chemistry that really affects what Baume' you can run, > with Chlorate limiting you to lower levels of Copper, than Hydrogen Peroxide. > > Rudy Sedlak > RD Chemical Company > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################