This measurement is not measurable per say. This means that the amount of solder needed will be only that amount needed to form a properly wetted solder fillet. In some cases, the acceptable solder fillet on class 1 & 2 products is so minimal that only that amount is what is needed to give you proper wetting physics. Barry Gallegos, PE Western Electronics, LLC 110 E. 43rd st. Boise, ID. 83714 P-208-377-1557 F-208-377-9836 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Roberts Jon Sent: Wednesday, September 27, 2000 1:00 PM To: [log in to unmask] Subject: Re: [TN] Wetted Fillet Also if hand soldering the "G" will not be as noticeable since the part termination will be down against the pads. With solder paste being applied first and the part placed on top a "G" will be more noticeable. Jon -----Original Message----- From: Sira Rikulsurakan [mailto:[log in to unmask]] Sent: Wednesday, September 27, 2000 9:05 AM To: [log in to unmask] Subject: [TN] Wetted Fillet Dear Technetors. Can anyone please explain me the definition of "Wetted Fillet" mentioned in chapter 12 of IPC-A-610C. For example Solder Thickness (Dimension G). Acceptable Class 1,2,3 = Properly wetted fillet evident. Thanks Mark. ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################