Before taking any action suggest you resample your pot, ensuring that you take a sample which is representative. Something like this: turn pot on allow to get to temp. After machine has been operating for an hour or so take a sample from the wave itself and chill it rapidly. If you really do have a high tin content like this you would most likely have already noticed it in results, would not need to have an analysis to find out. Quite an important question would then be how did it get to be like this?? Mike ----- Original Message ----- From: "Dave Girard" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, September 21, 2000 5:53 PM Subject: [TN] HIGH TIN WAVE SOLDERING > WHAT ARE THE CONSEQUENCES OF WAVE SOLDERING WITH SOLDER HAVING A HIGHER > THAN NORMAL TIN CONTENT (75-85%)? WAVE TEMPERATURE 485F (252C). > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################