Jim, Thanks for the quick response. It is good in a way to know we are not the only site to have seen a particular problem. Since this seems to be pretty rare (At least I had never heard of it before) I presume it must be related to the exact cooling behavior of the pot - size, shape, amount of solder, temperature, amount of insulation, otherwise everyone would have seen it. We have been covering the exit port of the machine, but in the last burp it fell down through the machine, hit the floor and splashed out where a person could have been standing. We will follow your lead and will now start to cover the source - the pot itself. Thanks. Bev -----Original Message----- From: Marsico, James [mailto:[log in to unmask]] Sent: Tuesday, September 26, 2000 2:16 PM To: [log in to unmask] Subject: Re: [TN] DENSE SMT ASSEMBLY Yes, I'm afraid I am serious... The board is 5 thousandths of an inch thick and is made of 6002 Rogers Duroid! Thanks, Jim M. -----Original Message----- From: Bev Christian [SMTP:[log in to unmask]] Sent: Tuesday, September 26, 2000 1:55 PM To: [log in to unmask] Subject: Re: [TN] DENSE SMT ASSEMBLY Jim, Are you serious?! Did you really mean the board is 5 thou thick or that the Teflon coating on the board is 5 thou thick or did you mean a 50 thou thick board? Bev Christian -----Original Message----- From: Marsico, James [mailto:[log in to unmask]] Sent: Tuesday, September 26, 2000 1:11 PM To: [log in to unmask] Subject: [TN] DENSE SMT ASSEMBLY Hello Technet: Well, the Electrical Engineers did it to me again! They're designing an assembly consisting of a Teflon surface mount board .005" thick, approximately 1.5 x 1.7", with 320 components! The component mix is mostly 0402's (resistors, caps and inductors) and 30 SOT-363s. Does anyone have any suggestions as how to automate this assembly process? Thanks in advance, Jim Marsico ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################