Al: We still use RMA for all tinning and secondary (hand) soldering operations. Bill Kasprzak Moog Inc. > -----Original Message----- > From: Alan Kreplick [SMTP:[log in to unmask]] > Sent: Wednesday, September 13, 2000 8:15 AM > To: [log in to unmask] > Subject: [TN] Subcontractors using RMA > > Hello technetters, > > A colleague of mine is looking for a contract manufacturer - in New > England - > that still uses RMA flux for some pth work. > > So, is there any CM out there still using RMA? > > > Al Kreplick > Sr. Mfg. Eng. > Teradyne, Inc. > 978-370-1726 > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################