Skipping phosphorous baths? Since the problem seems to be that phosphor is not solderable, eliminating the ability of a phosphor layer to build up during a hyperactive IG corrosion attack might just work. Perhaps a "Technetter" can expound on how to plate up nickel without the phosphorous. There are several studies collaborating with each other that low phosphorous levels in the nickel bath result in poor solderability and high levels result in good solderability. Thanks Ryan Grant Advanced Technology Engineer MCMS (208) 898-1145 [log in to unmask] > -----Original Message----- > From: Ingemar Hernefjord (EMW) [SMTP:[log in to unmask]] > Sent: Tuesday, September 12, 2000 8:37 AM > To: [log in to unmask] > Subject: [TN] BGA soldering and ENIG Phosphorous > > Got answers from Gerry, Stephan, Robert, Ryan and possibly some other, > again thanks a lot. But Steph, you made me confused, you said higher P > will eliminate aggressive mask attach from IG and reduce risk for building > up fragile P-enrichet layers between Ni/Sn intermetal and Ni. This is > opposite to what some other of you told me, namely that you should avoid > high P% baths. So, what do we prefer: little Phosphorous or much > Phosphorous. Please, don't say 'moderate'. > Or is it more a question of what IG we use (Biunno's article about > 'hyperactive IG corrosion on Nickel)? > > I can tell you the more simple solution if there is a problem: a company I > know just skipped phosphorous baths, and there were no more BGA soldering > problems. What do you think? > > Ingemar > Ericsson Microwave Systems > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################