Good day all, I need some help in deciphering a product specification, the product is Loctite Superbonder 495 What I am wondering is when the operator eventually drips some of this between circuit tracks is it going to cause me headaches. Here goes the properties Dielectric Constant, ASTM D 150 100 Hz 2.7 1 kHz 2.8 10 kHz 2.8 Dissipation factor, ASTM D 150 100 Hz <0.02 1 kHz <0.02 10 kHz <0.02 Volume Resistivity, ASTM D 257, V cm x 1016 - 0.6 Surface resistivity, V x 16 - 4 Dielectric Strength, ASTM D 149, kV/mm - 25 In a nutshell what do these numbers mean Thanks very much Jason ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################