Hi Bing! Test the solderability of the problem capacitors using specification ANSIJ-STD-002A to see if the solderability of the end terminations is an issue. Good Luck. Dave Hillman Rockwell Collins [log in to unmask] Milanie Racuya <[log in to unmask]>@IPC.ORG> on 08/16/2000 08:14:40 AM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to Milanie Racuya <[log in to unmask]> Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: [TN] Unsoldered joint on chip capacitor Hi guys, Just want to ask advice on what else to do on the unsoldered joints we are encountering regarding one vendor of the chip capacitor. We were using other vendors at that time then we used this one and it caused us a lot of headache. Same SMT machine settings, same solder paste, same ambient temperature and humidity. But using the new capacitor with the said vendor, we already had a problem on unsoldered joint. Does this mean that the solder paste we are using is not compatible with the component termination??? What we are doing right now is to drop a small amount of flux on the affected locations before processing it in the reflow. What advice can you still give me??? We are doing all what we can and yet, still the occurrence of unsoldered joints. Regards, Bing ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################