That's way too much baking... Your laminate may become brittle and the tin oxidised. You are using too much power to build boards at that point. We do not bake unless the boards are more then 6 months old or polyimide. We bake only once if required at all. Just my personal opinion, Alain Savard, B.Sc. Chemical Process Analyst -----Original Message----- From: Dieselberg, Ron [mailto:[log in to unmask]] Sent: August 10, 2000 6:14 AM To: [log in to unmask] Subject: Re: [TN] Baking Bare PCB's? Rick, I cannot speak for everyone, but this is what we have been using for about the last 15 to 17 years (or more). ""Bake the PWB for 3.5 +/- 0.5 hours at 185 +/- 25 deg. F and 27 in. Hg (685.8 torr) minimum. Rebake the board every 14 calendar days at 145 +/- 10 deg F for 12 hours minimum unless the PWB or PWA is not in work. If not in work, store in a dry Nitrogen box and rebake before the next soldering operation."" Hope this helps you. It did us! Ron Dieselberg BAE SYSTEMS Cincinnati Electronics Corp. -----Original Message----- From: Rick Thompson [mailto:[log in to unmask]] Sent: Wednesday, August 09, 2000 14:27 To: [log in to unmask] Subject: [TN] Baking Bare PCB's? I'm trying to establish some basic guidelines for the baking of bare PCB's that have potentially absorbed moisture due to unknown storage conditions and time. Are there any industry guidelines for this type of process or would someone mind sharing their general procedures? I thought I had read somewhere about times in the 2-8 hour range at 125 C but can't find that information anywhere. Thanks in advance. Rick Thompson Ventura Electronics Assembly 2665A Park Center Dr. Simi Valley, CA 93065 +1 (805) 584-9858 voice +1 (805) 584-1529 fax ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################