Hello TechNetters, I am trying to improve and automate the soldering process for a surface mount optical receiver. Presently it is being soldered by hand and although the results have recently improved, it would be desirable to automate to improve consistency. The major impediment to automation (and hand soldering) is the coplanarity of the leads. Over 60% of the parts have incoming coplanarity greater than 6 mils with a maximum over 10. Due to handling, by the time the part is placed onto the board and secured in place, nearly all the parts have greater than 6 mil coplanarity. Because of the extremely limited supply and uniqueness of these optical devices, the supplier(s) have not been as responsive to resolving incoming coplanarity issues as would normally be expected. I have tried a "point to point" automated solder system, but with the coplanarity issue, it does not presently appear a viable option. This seems to be an application where hot bar soldering might be a better solution. The parts have 6 leads at 50 mil pitch on both the "north" and "south" sides and 4 leads at 31 mil pitch on the "east" side of the component, all leads are solder dipped. I am not very familiar with hot bar soldering and would appreciate any input in regard to this application. Can all three sides be soldered at once? If hot bar appears viable, which vendors would you recommend? If other solutions spring to mind, please provide input. Obviously we will continue to work the coplanarity issue with the supplier(s) but I sure could use a solution now. Please respond to me directly or via the TechNet if you think it of value to the group. Any help is greatly appreciated. Thanks, Robert Furrow SMT Process Engineer Lucent Technologies 978-960-3224 [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################