Marc If you look at The deformation behaviour of Sn62Pb36Ag2 and its implications on the design of thermal cycling tests for electronic assemblies IEEE Transactions on Components, Packaging and Manufacturing Technology January 1999 pp. 71-79 you'll find what you need. Best regards Guenter Guenter Grossmann Swiss Federal Institute for Materials Testing and Research EMPA Centre for Reliability 8600 Duebendorf Switzerland Phone: xx41 1 823 4279 Fax : xx41 1823 4054 mail: [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################