>>> [log in to unmask] 07/26/00 02:57PM >>> Mike, I'm just a summer intern but I have all my books and references here with me. Could you give me your question again?? Thanks -Gary >>>>>>>>>>>>>>>>>>>>> Sure, no problem... We are experiencing problems with soldering of PLCC's. We find that a significant number of these devices are received from the vendor with non-coplanar leads. The lack of co-planarity causes open solder joints. Investigation has resulted in the knowledge that approximately 5% of the PLCC device we receive are not within the 0.004" co-planarity requirement. We find some to be out as far as 0.012". I cannot currently define the point at which the lack of co-planarity becomes an issue. The supplier is a major manufacturer of these devices. The parts are on tape and reel. We have inspected them prior to any processing at our facility, so we know that it is not a question of in-house handling, placement, etc. 1) Does anyone else see co-planarity problems with PLCC's? 2) What steps have you successfully taken to correct this problem, and what was the result? 3) Are there pieces of equipment I can put inline to screen <*gasp*> out these devices? 4) Any assembly or processing tricks you have used successfully to compensate? Thanks, Lang x5046 >>> [log in to unmask] 07/26/00 02:57PM >>> Mike, I'm just a summer intern but I have all my books and references here with me. Could you give me your question again?? Thanks -Gary -----Original Message----- From: Mike Lang [mailto:[log in to unmask]] Sent: Wednesday, July 26, 2000 2:43 PM To: [log in to unmask] Subject: [TN] PLCC Coplanarity... (or lack of) I got very little response to my coplanarity post, which leads me to believe that either no one else is having the problem, or no one else is using PLCC's, or... Is anyone out there using PLCC's without the coplanarity problems? Thanks, Lang x5046 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################