Hidee-ho ya'll!!! I just wanna say, I didn't mean to stir-up such a "hornet nest"...ya'll know me as a quiet sort of guy...right?...B^D Must say though, I've learned quite a bit about LPI soldermask processing, and that's what this list is all about. Thanks everybody!!! What has come out of this though, is that I'm determined to establish the means to be able to do our own cross-sections here. I want to either send somebody (or go myself) to the IPC-600F course to certify somebody to be able inspect and quantify what we get from our vendors. I just kinda' got thrown into the position of looking at the fabs we get, don't have any real training on this subject. But because my focus in the past has been in other areas, what little I know comes from what I read and what I learn from all of you. Wished I had more say as far as our purchasing department goes, but I don't. I could go on and on about the problems we have...we've got Philips equipment here but our buyers still buy parts from Digi-key...anybody that is familiar with what you get from Digi-key knows that you won't get anything that can be loaded on a tape and reel feeder, they'll be strips of parts...but that's a whole 'nuther thread... Hey, just want to say thanks for all the input!!! Still rejecting the boards though... -Steve Gregory- ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################