I have a need to place 1206 capacitors on pads design for 1812 components.
The caps are NPO (high quality).
The pad-to-pad dimension is very similar (within 0.003") for my 1812 pads
and 1206 pads, so that is not a concern to me. What is a concern is the width of
the pads which differ by about 0.060".
My question: Should I expect more defects or reliability issues by
using a pad which is 0.060" too wide on the 1206?
Thanks,
Lang
x5046