Got a question. Does Europe and Pacific Rim (off shore) process high volume linewidths of 125 microns (.005") on 35 micron (1 oz) copper foil (Innerlayers)? (Spacing is greater than 125 microns) I have a customer who eventually will want this and believes it may be an issue. David Hoover (aka, Groovy) (Somewhere near Disneyland California) ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################