it start to make sense now... if it is battery contact, it is usually either gold or SS (normally a little better SS than 304...so you will have corrosion on the battery pack but not on the assembly contact). Gold/SS (the contact on battery) coupling is not uncommon. Particularly for prototype...(besides, it is difficult to put SS on the board...)...If you using solder, you may have corrosion on the PWA due to solder/SS coupling. Battery contact should not be solder plated based on my understanding...(don't kill me, just my 2 cents)... jk At 02:32 PM 6/8/00 -0700, you wrote: >So here's the deal: > >They have two large circular pads (like about .750") that they use as battery >contacts. He says that this is the place that he has corrosion risk. I can't tell if >the corrosion risk is from battery leakage or environmental effects. Anyway, he says >that corrosion significantly impacts the battery life. > >ralph > >David Hillman wrote: > >> Hi Ralph! Can you provide more information on what the customer >> considers/experienced "corrosion" and what type of use environment he/she >> was talking about? >> >> Dave Hillman >> Rockwell Collins >> [log in to unmask] >> >> Ralph Richart <[log in to unmask]>@IPC.ORG> on 06/08/2000 11:55:26 AM >> >> Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond >> to Ralph Richart <[log in to unmask]> >> >> Sent by: TechNet <[log in to unmask]> >> >> To: [log in to unmask] >> cc: >> >> Subject: [TN] still confused >> >> We have answers.... >> >> So I had a long talk with my customer this morning to provide input >> based on the invaluable advice from you all. >> >> I said - "is there a specific reason for choosing 3-8u" of immersion >> gold over tin/lead solder?" >> He said - "absolutely, the gold provides corrosion resistance, the gold >> does not" >> I said - "even such a thin amount - only 3-8u"?" >> He said - "definitely, all we need is the coverage, the thickness is >> irrelevant" >> >> Is this true? >> >> Needless to say, we are rebuilding the parts as we speak. Rework sounds >> difficult to say the least, although I may try to come up with some >> scheme for fun as they have a bunch of boards that are no good right >> now. >> >> thanks for all the help..... >> >> ralph >> >> ############################################################## >> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c >> ############################################################## >> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in >> the body: >> To subscribe: SUBSCRIBE TECHNET <your full name> >> To unsubscribe: SIGNOFF TECHNET >> ############################################################## >> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional >> information. >> If you need assistance - contact Keach Sasamori at [log in to unmask] or >> 847-509-9700 ext.5315 >> ############################################################## > >############################################################## >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c >############################################################## >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in >the body: >To subscribe: SUBSCRIBE TECHNET <your full name> >To unsubscribe: SIGNOFF TECHNET >############################################################## >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional >information. >If you need assistance - contact Keach Sasamori at [log in to unmask] or >847-509-9700 ext.5315 >############################################################## > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################