Hi technetters, I'm hoping to find out a bit more about the effect of baking (at 45 deg. C) on boards with gold on nickel. I would be grateful for any info on the sibject, including times, temperatures and effects, such as passivation. Thanks, Richard TIlbrook ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################