Hi Dave, I have seen the "scaling" too. The ERSA rep said it was a defect, but not being a process guy, he could not explain why. He claimed that until the advent of the scope, the defect has gone unknown in the industry. For those who have not seen this before, it not a cold solder joint. Rather, it looks like an artists rendering of a cooling planet with plate tectonics. Actually, I believe it is quite common. I say this because I have seen it to a lesser extent on many brand new unprocessed BGA balls when viewed under a high powered scope. I have also seen it during cooling after reflowing solderpaste and viewing it through a microscope. Cooling tends to be rather uncontrolled and quite rapid. It appears as if the surface of the solder sphere solidified before the interior did. As the interior cooled, it shrank, pulling in the solidified exterior surface, causing the wrinkles. When I have watched it occur, it all happens in less than a second. There will be micro cracks, but they run normal to the surface. Since this is a natural physical phenomenon, I'm not sure how it is a defect. But I have not had time to investigate further. Maybe some of our other experts can explain. Thanks Ryan Grant Advanced Technology Engineer MCMS (208) 898-1145 [log in to unmask] > -----Original Message----- > From: Dave Simmons [SMTP:[log in to unmask]] > Sent: Monday, June 12, 2000 2:29 PM > To: [log in to unmask] > Subject: [TN] Scaling on PBGA Balls after reflow. > > Hi All, > > We are checking placement of some PBGA's. I have an ERSAScope on a demo, > and when viewing the solder balls/joints of the BGA there is some > "scaling" on the surface of the ball. > I was wondering what this scaling is a function of (e.g. to rapid > cooling, not hot enough, to hot during reflow?), and is it a defect I > should be worried about. I am not seeing this "scaling" on any of the > other parts (QFP100, 0603 chips) on the board. > Can anyone offer any advice? > Thanks > David << File: Card for David Simmons >> ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################