Hi there Phil, Rather than do it in house, and go through the cost of purchasing the equipment & adding to the work and skills required of your assemblers, why not get your PCB manufacturer to do it for you before you get the boards. I find that the additional 20p (or whatever) added to the cost of the PCB is usually less than the cost of hand application and all the messing about waiting for it to dry etc (and uses less mask). Simply create a Gerber file containing the areas that need it (or send them a hand done sample) and they can then sort it out. Its a standard service that they do. If you have any boards in stock, then it should not be a problem to send them back for the work to be done. You might find that any holes larger than 3mm are a bit hard to screen as the peelable resist goes down the holes & spreads about making a mess, it depends upon the consistency of the masking used. If the board is PTH, you could consider making any large holes (I.E. mounting's etc) non PTH & with a slight clearance in the land around the hole and then add several Via's around the land (but not where they may be under direct pressure) to enable any required continuity. If you need land visible for earthing, then you could put a 1mm+ slot into the bottom copper land so that the solder does not flow over it all. This way, they would not need peelable on big holes and they could go through the wave bath OK. Hope this helps - Matthew Lamkin. >-----Original Message----- >From: Phil Nutting [SMTP:[log in to unmask]] >Sent: Wednesday, May 10, 2000 8:50 PM >To: [log in to unmask] >Subject: [TN] Through Hole Wave Solder Mask Application > >To all, > >We are trying to cost reduce part of our through hole assembly. We build >high voltage power supplies and they don't lend themselves to SMT. The >boards have the standard LPI solder mask, but we need to mask some component >holes for components that are installed after wave solder. Currently we >apply ChemaskŪ Peelable solder mask by hand from an 8 fluid ounce bottle. I >know there are ways of applying a solder mask using a silkscreen. > >What equipment is needed? > >What mask material should I use? > >What support equipment do I need? > >Did I leave anything out? > >Thanks in advance for your input. > >Phil Nutting >Manufacturing Engineer >Kaiser Systems, Inc. >126 Sohier Road >Beverly, MA 01915 >ph: 978-922-9300 >fx: 978-922-8374 >[log in to unmask] > >############################################################## >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c >############################################################## >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in >the body: >To subscribe: SUBSCRIBE TECHNET <your full name> >To unsubscribe: SIGNOFF TECHNET >############################################################## >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional >information. >If you need assistance - contact Keach Sasamori at [log in to unmask] or >847-509-9700 ext.5315 >############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################