We use horizontal HASL machine. When I measured the thickness of tin/lead
    if the thickness was over 1um, the component of tin was 64~69%,
    if the thickness was under 1um (0.8~0.9um), the component of tin was always over 70%.
    (Tin/lead made-up in solder pot was 63+/-3%; 37+/-3%; board thicness was 1.6mm)
I did'nt know the reason why?
 
In the case of component of tin was over 70%, what will happen in
PCB Assembly manufacturing?
 
Any help would be appreciated.
 
Best regards,
Tri'.
 