I posted this question last week and unfortunately there was
only one person that responsed. I believe is topic is a major issue and that it
is crucial to our industry. So I will ask again. Once again we are being told of
glass cloth shortages for copper clad lamiantes. We are being told by the
suppliers that there will be allocations and increased prices. The reason for
this shortage is not very clear and I would like to know if others out there in
the PCB industry are being told the same thing and what type of price increases
are we looking at? Are all glass styles effected or are there just certain ones?
I would be happy to share any information that I have on this
matter.
Thanks