If you are doing X-ray with a dedicated operative / inspector plus keeping the image with the PCB then great, this tells you if there is a short, cracks, etc, whatever the quality of the x-ray machine allows you to do (and what it lets you do is proportional to cost). From my LIMITED understanding, this is an inspection tool, for testing each and every PCB where hidden faults (like under a BGA) are a possibility. For process control, it is advantageous to be able to look at the reflowed ball on a BGA. You inspect joints on every x PCBs to ensure the BGA balls are reflowing correctly, as compared to other joints on the PCB. The most publicised method of doing this is to use an "Ersascope" by ERSA. With all the bits and bobs, you can framegrab onto PC (supplied) and compare to a database thats supplied. The viewer can go 8 balls deep, the database can offer suggestions for your process. Before you go making any decisions, I believe that there are alternatives on the market. I cannot make a recommendation as I haven't looked that closely at the problem. Regards, Richard Tilbrook ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################