Ken: There are many factors to consider. We normally use Silicone Coating (Dow-Corning 2577) and on occasion we have had to use a polyurethane (Conethane CE-1155). First off, all spray guns, measuring cups, Zahn cups, stirrers, etc. must be dedicated for silicone coating. When we switch from silicone to the poly, we strip down all table tops, turn tables and even spray booth walls to totally eliminate all loose particles of silicone. The silicone basically forms a white snow flake like appearance on all surfaces.It is important to eliminate these loose particles. I have seen a single speck of silicone stick to a board surface and cause a non-wetted area around the speck approx. 1/8" diameter. It requires a lot of work to srcub down the affected area so that the poly material would stick. It is not unusual for our conformal coat operator to spend 4 - 6 hours in site preparation for using polyurethane in a silicone environment. I can't say the reverse is true because when we spray the poly material, it is a limited amount, therefore site preparation for going back to silicone is minimal. Bill Kasprzak Moog Inc. > -----Original Message----- > From: Ken Bloomquist [SMTP:[log in to unmask]] > Sent: Friday, May 19, 2000 9:37 AM > To: [log in to unmask] > Subject: [TN] Silicone Confromal Coating > > Hi TechNet, > > We have a customer that wants us to spray Silicone confromal coating on > their boards. We currently spray polyurethane and acrylic. > > My question is: Is there any problem adding Silicone to our process? What > art the things we need to consider in adding this process? > > Thanks, > > Ken Bloomquist > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################