Ivan Although some may not consider it logical, there is no reason why you should not do this PROVIDED that all the WS process is terminated before you start on the "no-clean" process. In fact, many use "no-clean" for rework after total WS production. Brian Ivan Barrios wrote: > Hello Technetters: > We are trying to go to No clean flux in our wave solder process. However, > we still run some of these products with water soluble paste in SMT. We > will still wash the boards after SMT to remove any of the residues from SMT > process. Any issues foreseen with mixing the two types of manufacturing > practices (No clean and Water soluble) in the same product? (corrosion, > reactivation of crystalized WS flux while it passes thru wave, etc) > Any and all responses are welcome > > Ivan Barrios > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################