Hi All! Probably too late to ask but I need some input for this weard problem. I got some connector with big leads that, with the unaided eye looks properly soldered. But if I look at it with the microscope at 10X, it looks like the fillet does not realy stick to the lead. The fillet end rather abrubtly (makes a rign) and it looks like there was no fusion between the lead and the solder. I hope my explanation is clear enough!!! JF ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################