Jason, Coming from years of our UIC Axial machine I would vote for all of the above! Actually it could happen at any of the process steps, however the most likely would be at the lead bending in the formers or at the lead cut process. That is where the 'pull' is put on the lead. However if the depth stop or the z-span is not correct the tips could actually come in contact with the glass and fracture it. Let me know if I can help any further. (A.I. is fun, aint it!!) Richard Hamilton Clemar Mfg. / Rain Bird [log in to unmask] > -----Original Message----- > From: Jason Larson, CET [SMTP:[log in to unmask]] > Sent: Thursday, April 27, 2000 4:32 PM > To: [log in to unmask] > Subject: [TN] auto insertion > > Hi Technet, > > This question is for those that are experts in auto insertion, > > At what phase of insertion (depth stop setting, lead shear, clinch, Z > span) > are you most likely to break a fragile component such as a glass pack > diode > or ceramic axial cap. > > We use a Universal VCD > > Thanks in advance, > > Jason > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################