Zach, I have an Engineering Handbook from a manufacturer of metering and mixing equipment. It lists the terms of viscosity and a comparison chart of common materials we are all familiar with, such as motor oil, honey, peanut butter. If this would help I'll fax a copy to you. Regards, Phil Nutting Manufacturing Engineer Kaiser Systems, Inc. 126 Sohier Road Beverly, MA 01915 ph: 978-922-9300 fx: 978-922-8374 [log in to unmask] -----Original Message----- From: zach crawford [mailto:[log in to unmask]] Sent: Thursday, April 20, 2000 4:58 AM To: [log in to unmask] Subject: [TN] : Viscosity Hi all, does anyone know of a valid source for viscosity data on liquids either over the internet or in any books. Looking for something with quick and easy access!! Cheers Zach ______________________________________________________ Get Your Private, Free Email at http://www.hotmail.com ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################