Hello Raj, We use a Kapton stencil from KJ Marketing. They work great. The release is far better than stainless and the other benefits are: -greater contrast visually from the paste (thus easier to spot plugging) -virtually no sag, therefore, better contact to pcb. -same or less cost than stainless. Try 'em out. Jason Gregory Production Manager Electrospec (713)784-4900 (713)784-1194 fax [log in to unmask] >>> Rajkumar <[log in to unmask]> 04/10 7:59 AM >>> Hi Technetters, Is there anyone out there using polymer stencils for printing solder paste? I would be interested if someone can share their experiences in printing with these stencils. Regards Raj ! ! ! ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################