Hi all, We are experiencing problems with a 6-way surface mount connector. The part in question is a Harwin part M22-634XX22R. And to a lesser degree the mating part M22-C107133C. The problem is that the joints do not appear wetted at all, the component legs seem to be sitting on top of the solder and the slightest force will cause the connector to fall off. The problem is currently being investigated by our manufacturing department, but I am keen to glean as much info as I can as to the possible cause. As is the first time with have used a surface mount connector, any advice would be most appreciated. I have sent this message to the TechNet forum, but I would be interested to hear from any pcb designers who have used the above parts, or similar parts and have experienced problems. Especially if you have had to make any changes to the recommended footprint to meet your assembly requirements. Best regards, Mark. Mark Holmes PCB Designer Helvar Merca Ltd. Hawley Mill, Hawley Road, Dartford Kent. DA2 7SY Tel: 01322 22 22 11 Fax: 01322 282 286 mailto:[log in to unmask] http://www.helvar.com