Dear Technetts, I have one custom design three leg SMT component. Two side leads (which are pretty massive and one middle center post). These leads are designed to create butt joints. Drawing specifies 0.004" coplanarity for all three leads. We are using 0.007" stencil. Now $1,000 question. I am using my life line and asking audience to help me. It seems, that center post doesn't create good solder joint. There are cases, when it seats only 0.001" deep in the solder and may break easily. I cannot use more than 0.007" stencil due to other component packages. I don't want to touch up each solder joint after reflow. What would you recommend? Please advise. Sincerely, Stella ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################